How To Weld A Cast Iron Bell. On the welding rod there is flux Special Graphite rich flux. Work on one inch at a time and allow about 45 seconds for the segment to cool down before moving on to the next one.
After every weld peen the bead tap it lightly with the round part of a ball pein hammer. Then you will drill and grind out a shape like U in the metal until it does not look like a hairline crack. For this repair I stick welded ca.
Using the methods discussed above weld the studs in place and cover the entire surface of the break with weld deposit.
There were two shops specializing in the work. For this repair I stick welded ca. After every weld peen the bead tap it lightly with the round part of a ball pein hammer. The two lower links are no problem because I will be welding directly to the steel axle tubes.